Evaluation of the effect of one-step self etching adhesives applied in pit and fissure sealing

SU Hong-ru, XU Pei-cheng, QIAN Wen-hao   

  1. Department of Oral Medicine, Shanghai Xuhui Dental Diseases Prevention and Cure Center. Shanghai 200032, China
  • Received:2015-10-15 Revised:2015-12-28 Online:2016-06-25 Published:2016-07-22

Abstract: PURPOSE: To observe the effect of three one-step self etching adhesive systems used in fit and fissure sealant and explore the feasibility of application in caries prevention in school. METHODS: Seven hundred and twenty completely erupted mandibular first molars in 360 children aged 7 to 9 years old were chosen. The split-mouth design was used to select one side as the experimental group, divided into A1(Easy One Adper), B1(Adper Easy One), and C1(iBond SE).The contra lateral teeth served as A2,B2 and C2 groups (phosphoric acid). The retention and caries status were regularly reviewed .The clinical effect of the two groups was compared using SPSS19.0 software package for Chi - square test. RESULTS: At 3 and 6 months, pit and fissure sealant retention rate in A1 and A2, B1 and B2,C1 and C2 group had no significant difference. At 12 months, sealant retention in A1 and B1 group was significantly lower than A2 and B2 group (P<0.05). No significant difference was found between C1 and C2 groups (P>0.05). At 24 months, sealant retention rate in A1, B1 and C1 group was significantly lower than A2, B2 and C2 group (P<0.05). The caries rate in A1and A2, B1 and B2, C1 and C2 group had no significant difference during different follow-up time (P>0.05). CONCLUSIONS: The clinical anticariogenic effect of three kinds of one-step etching adhesives and phosphoric acid etching sealant was similar .One-step self etching adhesive system was recommended for pit and fissure sealant to improve the students' oral health. The long-term retention rate of one-step self etching adhesive system was lower than the phosphoric acid method to long term observation is needed.

Key words: Pit and fissure sealant, Self-etching adhesive, Phosphoric acid, Retention rate